Maristop A Technical Data

Base Components

Prepolymer
Accelerator
Density at 25°C (g/cm³)
1.1
0.8
Viscosity at 25°C (mPa.s)
35
10
Quantity of accelerator added to the prepolymer (%)
0.5 - 10
Shelf life at 20°C (months)
6
12

 

Polymerised Product

 
Application temperature (°C)
15
25
Reaction time at 20°C with 10 % accelerator (min.)
1:15
0:45


The above data are values obtained in laboratory tests. They may vary according to site application conditions.
© Bautaxa 2001
Last updated 16-Apr-2001
If you find any problems on this page, please let me know:
webmaster@bautaxa.com